In theory both will have same UTS. But while testing, slight variation may be there due testing conditions.
--
-- 2010/12/16 Shaunak Upadhyay <shanupadhyay@gmail.com>
1) Material Specifcaiton: SA 516 GR 70
Size: 6.0 mm thk
300 mm Length x 300 mm Width
Process: GTAW
Consumable: ER70S-2
2) Material Specifcaiton: SA 516 GR 70
Size: 6.0 mm thk
300 mm Length x 300 mm Width
Process: SMAW
Consumable: E7018
Which test piece have more UTS in these two processes.
Regards,
Shaunak Upadhyay
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
regards,
Harish.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment