Wednesday, December 15, 2010

Re: [MW:8746] Regarding cutting process for high chrome material

You may use poly crystalline diamond cutting tool. You may consult Metatech Pune for diamond cutting tools.

2010/12/15 vinit vani <vinit_vani@yahoo.co.in>
Dear all
 
please go through the attached figure of hardfaced roller tyre. We want to cut the piece as shown in figure for failure analysis.
 
My query is-
1) what will be the suitable cutting process for High Chrome material?
 
2)Which parties in India specially in Mumbai offers such service?
 
Urgent reply with possible causes for this crack will be highly appretiated.
 
Thanks & Regards
 
Vinit

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
regards,
Harish.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...