RE: [MW:8639] Acceptance criteria in alloys in pmi testing below specified limits

Variation +/- 10% for base material, and +/- 12.5% for weld metal can be allowed

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shiv Dutt Mishra Mishra
Sent: Thursday, December 09, 2010 5:08 PM
To: materials-welding@googlegroups.com
Subject: [MW:8638] Acceptance criteria in alloys in pmi testing below specified limits

Dear All, can u tell me what is the acceptance criteria for the Ni,Cr
& Mo content below specified values in pmi testing in SS316 L
material.And which standard relates to it.How much deviation we can
accept. SDM


--
Thanks,
S.D.Mishra
Mob- 09589444897 (M.P./C.G.)
09766916581 (Maharastra)


Filtered by Hosted Filtering


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...