Thursday, December 9, 2010

[MW:8665] Welding of T/P 23&T/P 24 Material

Dear All,

Design Code: ASME BPVC SEC I

Welding Code: ASME BPVC SEC IX

I need your help as I am struggling in an unfamiliar territory. I have to weld the following materials. These material grades are totally unfamiliar for me. What are the precautions we have to take during fabrication of these materials? What would be the matching welding consumable to weld T/P23 to T/P 23 &T/P 24 to T/P 24?What would be the matching consumable to weld T/P 23 to T/P 24?Preheat and PWHT required or not? If yes, what would be the optimum range? It will be highly appreciated, if someone could provide some good literature on fabrication of these materials.

Cr-Mo Type

ASTM/ASME

DIN/VdTUV

EN

2.25 CrMoVW

T/P 23

HCM 2S

7 CrWVMoNb 9-6

2.25 Cr-1MoVTiB

T/P 24

7 Cr MoVTiB 10-10

7 CrMoVTiB 10-10

 
Thanks in advance

 

Regards,

 

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...