Thursday, December 23, 2010

[MW:8935] Material with impact test records.



-- Dear gents,
 
MERRY XMASS & HAPPY NEW YEAR  to all of you .
 
 I have a PQR, 316 L for sour service with impact test, at -196 C. It is a client requirement. But the material test certificates doesnt shows any impact test results.  it shows MEETS THE MRO 175 requirements.  This MTC is acceptable with out impact test? ,  Shall I do the impact test on the above material?  and if it meets the client requirements  shall we use the same material for all the production? seeks your valuable advise and opinion above matter.
Suresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...