[MW:8840] LOP in MIG Welding Qualification

Dear All,
Recently I have noticed this in one company and want to share with you.
It was a procedure Qualification as per sec IX.
Process is GMAW (MIG).
Plate thickness is 25mm.
Wire Dia is 1.2mm
Root gap is 2.5mm.
Current was 75 A.
After root pass welding found LOP for almost total length.
What is the best way to avoid LOP.
 
Regards,
C.Muniyandi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...