Saturday, December 18, 2010

[MW:8787] ACCEPTANCE STANDARD FOR PRESSURE VESSELS

Dear Sir,

In pressure vessel fabrication during welder and welding
qualification, which acceptance standard we should follow for
mechanical test and weld visual inspection whether ASME SEC VIII OR
IX.

--
Thanks & Regards
M.Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...