[MW:8732] ASTM E45 method D (How to determine?)

I was facing some difficulties when performing inclusion test
accordance to E45method D

Normally the test sample is carbon steel.

1. I polished the test sample's surface to 0.06µm.
2. observed the surface under 100X.

The difficulties or doubts that i'm facing:
1. The sample will rust, some dots on surface, is very hard for me to
determine which 1 is inclusion.
2. How to differentiate silicate and sulfide? (refer to Plate I-r)
3. How to differentiate aluminate and oxide?
4. after i polished, all the black dots or lines on surface are
inclusions?
5. Is there any link or good book for reference.


Thanks in advance. :)


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...