[MW:8667] RE: 8643] Thickness calculation for weldolet

The answer is a definite yes. The procedure has to support the thinnest
member of the pressure retaining component.
I was made aware of this during my three year stamp renewal.

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Srini
Sent: Thursday, December 09, 2010 1:52 PM
To: Materials & Welding
Subject: [MW:8643] Thickness calculation for weldolet

Hi,

How do we calculate the thickness of the weldolet for welding
procedure qualification? Code is B31.3 and ASME SECIX. Weldolet is 8"
SCH40 Bonney forge. So is the thickness (B-C)/2 ie 21mm? Does the
procedure qualification has to support base material thickness of
21mm. The pipe is 8" SCH40. Which section of B31.3 or SEC IX would
address the requirement for this attachment weld between pipe and
weldolet?

Thanks for your help.
Srini

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own
decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...