kindly mention what type of adhesion test is going to conduct?(cross
cut/pull-off)and please mention the paint system .if it is silicone
based we cannot do pull off test i think and standard for code is ISO
4624 and for cross cut test ISO 2409.after the top coat pull off test
is required
Haseeb
On Dec 8, 10:10 am, Sundaram Sundaram <nss2...@gmail.com> wrote:
> Hi friends,
>
> For conducting a ashesion test in the structural
> steel 3coat paint system,which code is to be used .pls guide me.
>
> with thaks,
> sundaram
--