[MW:8494] Pre heat and post heat for welding Bisalloy strips to 4140 HT (Heat Treated)

Can someone please assists me with the welding process I require to know the pre heat and post heat requirements to weld strips of Bisalloy 12-HX450 grade to  4140 HT material. The use of this will be for the drilling industry.

 

I hope someone can help

 

Look forward to your replies

 

Regards,

 

 

Alan Jacklin

 

Description: LOGO

P. 07 3382 6600   F. 07 3382 6611

E. alanexpresshyd@bigpond.com

 

1 comment:

oh said...

i have a question

what is the difference of

1)after welding then straight away go for post heating

2)after welding , then pause welding (welding duration too long) then when welding is done(after 2 days of welding ) then only proceed to post heat.

will the paused gap affect anything?