Monday, November 15, 2010

RE: [MW:8280] new attached file-Electrode calculation

What was the welding process that these numbers were derived from??

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthik
Sent: Friday, November 12, 2010 11:56 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:8233] new attached file-Electrode calculation

 

Hi,

This attached file is a good one.

 

Thanks & Regards,

 

(Karthik)

 

Karthikeyan.S

QA/QC Manager

Getabec Energy Co.,Ltd.

379,Moo6,Soi8,Nikhomphatana,

Rayong-21180,

Thailand.

Phone: 0066 38 897035-8 (Off)

Fax: 0066 38 897034

Hand Phone: 0066 892512282



--- On Sat, 11/13/10, Shadab Alam Ansari <ansari@ghi.com.sa> wrote:


From: Shadab Alam Ansari <ansari@ghi.com.sa>
Subject: [MW:8230] Electrode calculation
To: materials-welding@googlegroups.com
Date: Saturday, November 13, 2010, 11:50 AM

Dear All,

How to calculate weight of electrode required for a joint?

What are the factors considered for calculating the Electrode consumption for a particular joint and what are their coefficient factors?

Thanking you,

Best regards,

Shadab

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...