Re: [MW:8251] Tensile test specimen

Kumar,
 
The basic reason of shape given to the specimen is because spec requires so. It is so to concentrate stress in the region we want to study. If full specimen is of the same size, like reinforcement bars are tested, we wont be able to focus on a specific region to study the mechanical properties as it may break in the grip region and test would be wasted.
 
Regards

On Sat, Nov 13, 2010 at 9:43 AM, vinod kumar <vinodmylaraiah@gmail.com> wrote:
Dear peers,
I need some information regarding the shape of the Tensile Test specimen.(As per ASTM A370)
When we are doing the tensile test, why we need to take the sample in the form of Dumbell or Shouldered specimens?
Is the shape is only for the grip purpose?

--
Thanks and Best regards

Kumar

"Never Explain yourself to any one Because the person who likes you doesn`t need it, and the person who dislikes you won`t believe it."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...