Dear Mister Soman,
 
Please google on alutite.
Alutite is a soldering method for repairing aluminium, which can be done wirh a normal flame what means lower heatinput.
If you cant find it please let me know.
 
Best regards,
 
Huib van den Tol

2010/11/11 <donboscomarine@vsnl.net>

November 11, 2010

 

Dear Friends,

 

The attached is a report of the repairs carried out on a Vintage Car's Engine's cylinderhead and the continuing problems of the same. The material is cast Aluminium and being a vintage car, replacements are not available. Cutting the present cylinderhead for making moulds for casting not acceptable to owner due to the risk of losing the cylinderhead for good ! We have described the problem and seek advice about Probable Solutions. 

Thanks in advance & B. Rgds.  

G. A. Soman

Principal

 



DON BOSCO MARITIME ACADEMY
Premier Automobiles Road,
Kurla West, Mumbai 400070
Tel:  (022) 2504 1585 / 2018; 25036344.  Fax: (022) 2504 0682
Email:  donboscomarine@vsnl.net
Website: www.dbma.in
Mobile No:  9819451277

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...