Dear Mr. K.Babu,I couldn't find the P No. and Gr. No of the material(ASTM A 519 Gr.4130) which you have mentioned in your query.The following ASTM A 519 Grades are listed in ASME BPV SEC IX, 2010 Edition.
Spec NoType or Grade
UNS No.
Minimum specified tensile strength
Welding
Brazing
ISO 15608 Group
Nominal Composition
Product Form
P.No.
Gr.No.
P.No.
ATM A 519
1018HR
G10180
…
1
1
1
1.1
C
Tube
ATM A 519
1018CW
G10180
…
1
2
1
1.1
C
Tube
ATM A 519
1020HR
G10200
…
1
1
1
1.1
C
Tube
ATM A 519
1020CW
G10200
…
1
2
1
1.1
C
Tube
ATM A 519
1022HR
G10220
…
1
1
1
1.1
C
Tube
ATM A 519
1022CW
G10220
70
1
2
1
1.1
C
Tube
ATM A 519
1025 HR
G10250
55
1
1
1
1.1
C
Tube
ATM A 519
1025CW
G10250
75
1
2
1
1.2
C
Tube
ATM A 519
1026 HR
G10260
55
1
1
1
11.1
C
Tube
ATM A 519
1026 CW
G10260
75
1
2
1
11.1
C
Tube
Regards,LimeshOn Wed, Nov 10, 2010 at 11:28 AM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
--HiSome one help me to have the P NO/GP NO for the above material in latest edition of ASME Sec IXI don't have latest edition of ASME, as this material in earlier editions as unlisted one.Thanks & Regards,K.BabuSingapore
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Thursday, November 11, 2010
Re: [MW:8199] ASTM A519 Gr.4130 - P No/ GP No. ? in ASME 2010 Ed.
Hi Limesh
Thanks for the info.
As per AWS B2.1 it is falls under M no.: 11B/ Gp no.: 9
Regards
K.Babu
Singapore
Subscribe to:
Post Comments (Atom)
[MW:34920] Tubesheet Hole step
Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP -- https://materials-...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment