Wednesday, November 10, 2010

Re: [MW:8181] ASTM A519 Gr.4130 - P No/ GP No. ? in ASME 2010 Ed.

Dear Babu,
It does not fall under any P- No. or Group No.
This is an unassigned material.
If you are fllowing API 6A, 16 C codes, they allow to group yourselves with similar materials but not equivalent such as AISI 4140/ ASTM A 487 etc.
Thanks and Best Regards,
K.Rajagopal
On Wed, Nov 10, 2010 at 11:28 AM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Hi
 
Some one help me to have the P NO/GP NO for the above material in latest edition of ASME Sec IX
 
I don't have latest edition of ASME, as this material in earlier editions as unlisted one.
 
Thanks & Regards,
 
K.Babu
Singapore
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...