Monday, November 8, 2010

Re: [MW:8137] PT LEVEL 1 QUALIFICATION

It is not exactly like that.
in the paragraph 4.3.1 of SNT-TC-1A 2006 it is stated that level I can perform:
"specific evaluation for acceptance or rejection determination, according to written instructions and to record results. The NDT level I shall receive the necessary instruction and supervision from a certified NDT level II or III individual".
The key words are instruction and supervision

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04

Inactive hide details for asad azmi <azmiasadayub@gmail.com>asad azmi <azmiasadayub@gmail.com>


    asad azmi <azmiasadayub@gmail.com>
    Sent by: materials-welding@googlegroups.com

    07/11/2010 11:49

    Please respond to
    materials-welding@googlegroups.com

To

    materials-welding@googlegroups.com

cc


Subject

    [MW:8121] PT LEVEL 1 QUALIFICATION

Ref


Dear All,
 
Greetings.
 
Please inform me about the Standard and para which states that personnel performimg Liquid Penetrating Testing shall be Level 1  & Person resposible for Interpretaion of PT shall be Level II
 
Thanks and Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...