In addition to Mr Goswami"s suggestion ,genrally Hydrotest is not carried with scale
Regards
 
Hegde


From: pgoswami <pgoswami@quickclic.net>
To: materials-welding@googlegroups.com
Sent: Wed, 3 November, 2010 6:38:34 PM
Subject: [MW:8052] RE: 8051] effects of scales on corrosion rate

Hello Asad,
 
These scales would be harmful.There may not be issues during fabrication, but definitely during service,such as:-
  • Loose/soft scales may may get removed and clog the piping/valves and strainers downstream
  • Hard scales would stick to the vessel surface.If the operating media is corrosive, which any process fluid is always to certain degree, then it would ideal sites for crevice/pitting corrosion.
If required it would be advisable to get your client involved and influence the fabricator to get the scales removed completely.
 
Thanks
 
Pradip Goswami,P.Eng.
Welding & Metallurgical Specialist & Consultant
Email-pgoswami@sympatico.ca,
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: Wednesday, November 03, 2010 6:34 AM
To: materials-welding@googlegroups.com
Subject: [MW:8051] effects of scales on corrosion rate

Dear All,
 
Greetings.
 
During inspection  of the internal surface of the CS vessel before despatch, heavy scales some loose and some hard  (adhered to surface) were observed  on the 33mm thick dished head. The Vessel  is PWHTed. Dished head is HOT FORMED.
 
 
pls refer attachment for your reference.
 
Contarctor is not willing to remove the scales completely. whether the scales which are adhered to surface are also need to be removed.
 
Pls suggest whether the vessel can be accepted with scales. what is the effect of scales on the metal surface. is it going to affect service requirement.
 
Thanks and Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...