Monday, November 1, 2010

RE: [MW:7996] No of Welders

As far as ASME IX is concerned please read carefully the notes of QW-251.(a) and of QW-452.1(b)

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04

Inactive hide details for César Alexis Viteri Pérez <alexis_viteri@hotmail.com>César Alexis Viteri Pérez <alexis_viteri@hotmail.com>


    César Alexis Viteri Pérez <alexis_viteri@hotmail.com>
    Sent by: materials-welding@googlegroups.com

    30/10/2010 20:27

    Please respond to
    materials-welding@googlegroups.com

To

    <materials-welding@googlegroups.com>

cc


Subject

    RE: [MW:7949] No of Welders

Ref


Dear Members,

Is it acceptable to qualify 2 welders (API 1104 - 6G - one by side) per cupon (down from 8" NPS) or not ?
Is it acceptable to qualify 2 welders (ASME IX - 6G - one by side) per cupon (down from 12" NPS) or not ?

Thank and regards


Date: Sat, 30 Oct 2010 10:37:56 +0000
To: materials-welding@googlegroups.com
Subject: Re: Re: [MW:7943] No of Welders
From: drpaulosejohn@rediffmail.com

Dear Mr. Arun,

Minimum number of welders to be qualified by one WPS is - One welder. The welder who performs the PQR coupen welding is automatically becomes qualified. Please refer 2nd para of QW 301.2 of Section IX:2010 and para 621 of API 1104:2007.

Regards,
Dr. Paulose John
QA/QC Manager,
Unisis Engineering,
Saudi Arabia
.
On Sat, 30 Oct 2010 14:15:07 , No ID Specified wrote
To my knowledge there is no limit for number of welder qualification upon one WPS, You can qualify as many as per to the requirement for your project.



Here By,

P.BalajiRajan,
-------Original Message-------

From: Arun Das
Date: 10/28/10 17:39:52
To: materials-welding@googlegroups.com
Subject: [MW:7911] No of Welders

Sir,

Minimum number of welders to be qualified upon one WPS is mentioned in SEC 1X or API 1104.
We are using PIPE,16"X0.375"WT STD SCH API 5L X52

Thanks in advance

with regards,

Arun S Das


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...