Hardenss for P1
Max HB:220 Max HV:250

Hardenss for Sour water and other corossion services P1 & P9
Max HB:200 Max HV:240

regards

shahul hameed

ahmed wrote:
> Dear Friends,
>
>
>
> I want to know that
>
>
>
> What is max & Min value of Hardness BHN for NACE C.S. material A106
>
>
>
> Thanks to all
>
>
>
> Waiting for ur reply
>
>
>
> Best Regards,
>
> Shaikh Ahmed . k .
>
> QA/QC Engineer
>
> COSTAIN ABU DHABI COMPANY.W.L.L
>
> (A division of Costain Oil & Gas Process Limited, Manchester, UK)
> P.O. Box no: 3069
> Abu Dhabi-Das Island
> United Arab Emirates
> * Email :ahmed@costaindas.ae
>
> Mobile: +971-567090644
> * Tel: +971-2-6063850 (Ext:216)
>
> Please visit <http://www.costain.com/> www.costain.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...