Wednesday, November 3, 2010

[MW:8051] effects of scales on corrosion rate

Dear All,
 
Greetings.
 
During inspection  of the internal surface of the CS vessel before despatch, heavy scales some loose and some hard  (adhered to surface) were observed  on the 33mm thick dished head. The Vessel  is PWHTed. Dished head is HOT FORMED.
 
 
pls refer attachment for your reference.
 
Contarctor is not willing to remove the scales completely. whether the scales which are adhered to surface are also need to be removed.
 
Pls suggest whether the vessel can be accepted with scales. what is the effect of scales on the metal surface. is it going to affect service requirement.
 
Thanks and Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step