[MW:8034] effect of PWHT Temperature at 600 DEG CELSISIUS ON SS 316L

Dear All,
 
Greetings.
 
Contractor is doing PWHT of the Carbon Steel Vessel along with  SS316L  INTERNALS ( BEAMS, CHANNELS) Bolted with the Vessel.  PWHT temperature is 600 DEG CELSIUS.
 
Pls  suggest me whether it is allowed. what will be the effect on mechanical proerties/corrosion ressiatnce  proerties of SS 316L becuase of the PWHT Temperature.
 
Thanks in advance for your valuable suggestions.
 
Regrads

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...