Monday, November 1, 2010

[MW:7977] consumable containing more than 1% nickel in sour environment

Dear All,
 
Most of the client specification banned usage of consumable containing more than 1% nickel in sour environment.What would happen if we use consumable having more than 1% nickel?
If any damage will be the result,how it happening?
 
 
Regards,
 
Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.