Dear Dr.John,
 
As a custom for above 12" pipe we will be using 2 welders for the welding process. It is so done because of heat input and distribution factors I beleive, but my question was that do this is stated as mandatory in any of the codes or standards.
I am having 1104 20 th edition of November 2005 with me. API 1104:2007. is the modifications??
 
Thanks and regards,
 
Arun S Das



From: Dr. Paulose John <drpaulosejohn@rediffmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Sat, 30 October, 2010 4:07:56 PM
Subject: Re: Re: [MW:7943] No of Welders

Dear Mr. Arun,

Minimum number of welders to be qualified by one WPS is - One welder. The welder who performs the PQR coupen welding is automatically becomes qualified. Please refer 2nd para of QW 301.2 of Section IX:2010 and para 621 of API 1104:2007.

Regards,
Dr. Paulose John
QA/QC Manager,
Unisis Engineering,
Saudi Arabia
.
On Sat, 30 Oct 2010 14:15:07 , No ID Specified wrote
To my knowledge there is no limit for number of welder qualification  upon one WPS, You can qualify as many as per to the requirement for your project. 
 
 
 
Here By,
 
P.BalajiRajan,
-------Original Message-------
 
From: Arun Das
Date: 10/28/10 17:39:52
Subject: [MW:7911] No of Welders
 
Sir,
 
Minimum number of welders to be qualified upon one WPS is mentioned in SEC 1X or API 1104.
We are using PIPE,16"X0.375"WT STD SCH API 5L X52
 
Thanks in advance
 
with regards,
 
Arun S Das

 
FREE Animations for your email - by IncrediMail! Click Here!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...