Re: [MW:7964] Longitudinal weld seam staggering

Pl refer DNV OS F101 for Pipeline and API RP 2A for structural . Min 3" seggration . Most of the project specifications give the requirement , some time the staggering in top by 90 degree .

Best Regards,

Francis Lobo
----- Original Message -----
From: (PBR)P.BalajiRajan
To: materials-welding@googlegroups.com
Sent: Sun, 31 Oct 2010 00:57:28 +0530 (IST)
Subject: [MW:7959] Longitudinal weld seam staggering















Dear colleagues

 In any code details given regarding Longitudinal weld seam staggering requirements of adjoining pipes if so please forward,


Here By,

 

P.BalajiRajan,

 

 
FREE Animations for your email - by IncrediMail! Click Here!



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...