Re: [MW:7956] PWHT

Is it allowed/accepted practice for PWHT of matl combination P1+P5A, if so what is the temp, Mr Goswami
Thank u
Pandithan

On Wed, Oct 27, 2010 at 4:33 PM, Brl Pp <refazosaris@gmail.com> wrote:
Good morning,

Please see below the data of piping line for erection:

- Diameter of pipe: 48"

- Produced: liquefied natural gas.

- Piping class: D41A

- Piping thickness: 38mm.

- Weldolet thickness : 15mm.

- Design code: ASME B31. 3. 2008 Edition.

- PWHT: By code.

According to your experience, for this case we use the PWHT?

If yes, please share your experience. Thanks in advance.

My best regards.


Redouane (Project engineer)
Algeria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...