Thursday, October 28, 2010

Re: [MW:7916] About electrode

Vishal,

The SMAW, or fully Shielded Metal Arc Welding is a process where the filler metal is coated or shielded with the flux coating, 
Submerged Arc Welding is a welding process where the filler weld metal is submerged under the flux, be it recyclable or not and Gas Tungsten Arc Welding is a welding process where the shield is in the form of gas. Each is a different process. If we were to use coated flux metal for welding, it will always be called as shielded metal arc welding. Do not confuse SMAW with other welding processes.

On Thu, Oct 28, 2010 at 2:21 PM, VIshal Sapkale <sapkalevishalv@gmail.com> wrote:
Dear all,


i hv simple que.

we used coated electrode for SMAW so why don't we use coated filler wire for SAW & GTAW


Regards,
VIshal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
This message originated from the Internet. Its originator may or may not be who they claim to be and the information contained in the message and any attachments may or may not be accurate.

This email transmission is intended solely for the named recipient(s). It may contain confidential and/or privileged information.If you are not the intended recipient, note that disclosing, copying or distributing it may be unlawful. Please notify the sender immediately if you have received it by mistake, and delete it from your system.
Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.

"SAVE PAPER - THINK BEFORE YOU PRINT!"

Regards,

~ DEVARAJAN RAMASAMY~

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...