Dear Kiran

Herewith i have attached some useful files containing the welding procedures on the cast irons including SG iron also. Moreover, you can find another file regarding the UTP (Germany) welding consumables for Cast Iron. UTP is a company of 100 years old Bohler Welding Group based in Austria, a world leader in providing welding products and solutions.

If you are in india, u can contact Bohler Welding Group India Ltd, of which head office is located in mumbai, (www.bohlerweldinggroupindia.com) for further queries.

Thanks and Regards,

M.SarojKumar
Kingdom of Saudi Arabia.
Mobile: +966 566205444

On Mon, Oct 25, 2010 at 2:48 PM, Panshetty Kiran <kpanshetty@forbesmarshall.com> wrote:

Hi All,
Can any body Suggest me the welding of S.G.Iron (EN-JS 1025 / ASTM A 395) ?
Pl mention the standard,Filler Materila details & procedure.
 
Regards,
Kiran Panshetty,
 
 
******************************************
" Call 92256 37451 - Your helpline for everything in Steam "
DISCLAIMER:This e-mail message is proprietary to Forbes Marshall and is intended solely for the use of the entity to whom it is addressed. It may
contain privileged or confidential information exempt from disclosure as per applicable law. If you are not the intended recipient or
responsible for delivery to the intended recipient,you may not copy,deliver, distribute or print this message. If the contents are unrelated to
the Company's normal business activity it may be treated as personal views of the sender. The message and its contents have been virus checked.
but the recipients may conduct their own. FM will not accept any claims for damages arising out of viruses.
*******************************************

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...