to control the dft first you have to know the paint type, if it is a high build or not and most safe is first paint on the test panel and from that you can calculate no. of passes required to get the correct dft

Haseeb
KSA

On Wed, Oct 27, 2010 at 10:33 AM, Sundaram Sundaram <nss2410@gmail.com> wrote:
Thanku for your reply Mr.Gole.The primer DFT- 75microns,midcoat coat- 75 microns,final coat- 75 microns.overall 225 microns.Most of the times the total DFT is exceeding 225microns and how to control this.Can you give some more clear picture,pls


On Wed, Oct 27, 2010 at 11:15 AM, BHARAT GOLE <bharatgole@hotmail.com> wrote:
If surface profile is more than acceptable limit then it may cause for rust rashing i.e high peaks may expose after paint curing/contraction will be rusted.
Actaully it depend upon the so many factors such as whole paint syetem and DFT etc

Bharat B. Gole

 

 





> Date: Tue, 26 Oct 2010 22:58:41 -0700
> Subject: [MW:7857] Surface preparation and coating
> From: nss2410@gmail.com
> To: materials-welding@googlegroups.com

>
> Dear friends,
> Blasting Grade required - SA2.5
> Surface profile required - 40 - 70microns
>
> If the surface profile crossing the required limit 70-
> 80microns then what will the effect on painting and what is the
> reference code.Please guideme
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...