Re: [MW:7860] EXCESS PENETRATION

Dear;
         you can refer sec 341 of b 31.13 for excess penetration.


From: KASHKOUSHA <kashkousha1@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Mon, October 25, 2010 7:10:01 PM
Subject: Re: [MW:7791] EXCESS PENETRATION

 Dear P.Mahendran
thanks for prompt reply but what clause no in b31.3
 
H.KASHKOUSHA



From: mahendran p <pmahe_79@yahoo.co.in>
To: materials-welding@googlegroups.com
Sent: Mon, October 25, 2010 3:15:07 PM
Subject: Re: [MW:7788] EXCESS PENETRATION

Dear Kashkousa,
                         Its depends on the wall thickness.
 
for Example, if wall thk is
<=6 mm   then EP is 1.5mm
>6 < =13mm the EP is 3 mm
 
 
Thk & rgds,
P.Mahendran
 

--- On Mon, 25/10/10, KASHKOUSHA <kashkousha1@yahoo.com> wrote:

From: KASHKOUSHA <kashkousha1@yahoo.com>
Subject: [MW:7784] EXCESS PENETRATION
To: materials-welding@googlegroups.com
Date: Monday, 25 October, 2010, 6:17 PM

dear all
what is the acceptance criteria of excess penetration in ASME B31.3
THANKS
 H.KASHKOUSHA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...