Wednesday, October 27, 2010

RE: [MW:7859] Surface preparation and coating

If surface profile is more than acceptable limit then it may cause for rust rashing i.e high peaks may expose after paint curing/contraction will be rusted.
Actaully it depend upon the so many factors such as whole paint syetem and DFT etc

Bharat B. Gole

 

 





> Date: Tue, 26 Oct 2010 22:58:41 -0700
> Subject: [MW:7857] Surface preparation and coating
> From: nss2410@gmail.com
> To: materials-welding@googlegroups.com
>
> Dear friends,
> Blasting Grade required - SA2.5
> Surface profile required - 40 - 70microns
>
> If the surface profile crossing the required limit 70-
> 80microns then what will the effect on painting and what is the
> reference code.Please guideme
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...