 dear eng / mostafa
  please find attached catalog of intersted mateiral and include the welding procedure and heat tratment and filler metal . i hope to help you .
Yours sincerely,

QA/QC Eng.
ibrahim mohamed
petrojet -egypt
Tel




From: Eng/ Mostafa Kamel Hussein <mkh_200@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Sun, October 10, 2010 2:18:37 PM
Subject: [MW:7472] X20CR MO V12 1

what is the suitable electrode SMAW for X20 CR MO V 12 1

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...