Please comment on the following issue.
 
As per BS EN 10225, S420G2+M--thickness less than 40mm should have a tensile strength of 500 to 660MPa. Material test certifactes shows a vaue of 623MPa. This material is used for welding procedure qualification test where the tensile strength reported is 550Mpa. My collegue who is reviewing the WPS\PQR says that he will reject the WPS\PQR because tensile value of PQR test specimen is less than 623MPa. My opinion is that the PQR test specimen meets BS EN 10225 and so should be accepted.
 
Please comment on this issue. 

--

With Regards.
SGR

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...