Saturday, October 30, 2010

[MW:7947] QW 423 & QW 424(P.no) conflicts.... Clear me.

Dear All,
 
1)if P.no is changing, For example from P.no X to P.no Y, either we have to go for new WPS & new PQR or not, Clear me.. (Same Process)
 
&
2) If base material is changing within P.NO 1,  example, A106 to A36. Either i have to go for new PQR or not, & welder to be qualified for tat base material changing within P.no. 1 or not? (Same Process)
 
& 3) one welder got qualified in P.No X, is he only qualified to weld tat P.No only, am i correct or not... (Same Process)
 
Pl clear me about above three...

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...