Bevel angle is not an essential variable under ASME Sec IX but is an
essential variable under AWS D1.1.

If I were going to use an angle drastically small than 37.5, I
personally would qualify my welding procedure using that angle to
simulate production welding.

On Oct 26, 2:57 am, Sadique Sheikh <sadiq.m...@gmail.com> wrote:
> Dear All,
> In piping different bevel angels are used like 37.5, 32.5 etc.
> What are the criteria to decide bevel angle in piping?
> Does it depend upon wall thickness and pressure of piping?
>
> Thanks & Regards,
> Mohd. Sadique Sheikh
> BUREAU VERITAS

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...