this is not addressed in codes that I know of.

With GTAW, the weave width depends upon the size of the cup when
"walking the cup" and should not have any affect on the weld in that
you can control heat with travel speed with GTAW.

On Oct 16, 6:02 am, limesh M <limes...@gmail.com> wrote:
> *Dear All,*
> **
> *I heard about weaving ,which is applicable in SMAW.If I am crossing the
> weaving barrier as per manufacturer recommendation,ie,  2.5 X dia of
> electrode or 3 X dia of electrode what would happen?*
> **
> *Is weaving applicable in GTAW? If applicable what would be the weaving
> range?*
> **
> **
> **
> *Regards,*
> **
> *Limesh*

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...