Wednesday, October 27, 2010

[MW:7874] PWHT

Good morning,

Please see below the data of piping line for erection:

- Diameter of pipe: 48"

- Produced: liquefied natural gas.

- Piping class: D41A

- Piping thickness: 38mm.

- Weldolet thickness : 15mm.

- Design code: ASME B31. 3. 2008 Edition.

- PWHT: By code.

According to your experience, for this case we use the PWHT?

If yes, please share your experience. Thanks in advance.

My best regards.


Redouane (Project engineer)
Algeria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments: