Paul

 

Strickly there is no equivalent and it has to be treated in ASME as unassigned material. However if you have the full test certificate for all practical purposes you can group it.

 

Please contact me directly in the office to discuss as I find it strange that as a member of SAIW you don’t make use of the services

 

Regards

 

John du Plessis

Technology Manager

 

Tel: +27 (11) 298 2100

Tel: +27 (11) 298 2103 (Direct)

Fax: +27 (11) 836 6014

Mobile:+27  82 883 4970

www.saiw.co.za

 

This email and any files transmitted with it are confidential and may be legally privileged. They are intended solely for the use of the individual or entity to whom they are addressed. Access to this e-mail by anyone else is unauthorised, and any disclosure, copying, distribution or other use of this e-mail is prohibited and may be unlawful. We will not under any circumstances have any responsibility or liability arising out of or in connection with any unauthorised use of this e-mail. If you have received this email in error please notify the sender before deleting it.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Paul Osikwemhe
Sent: 19 October 2010 02:55 PM
To: materials-welding@googlegroups.com
Subject: [MW:7651] ASEM equivalent of EN10025 S355JR

 

Dear all I have two questions (1) I want to know the ASEM equivalent of EN 10025 S355JR

                                                         (2) Can I use ASEM PQR for the EN 10025 S355JR

Regards

Weld map

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...