Dear all,

      Here by i am araising one question which i am in need of some clarification.

 

I am having a vessel to be repaired and that vessel is a carbon steel and inside with stainless steel material. That vessel is a PWHT vessel. Now we are going to repair that vessel, due to corrosion. But after welding we cannot do PWHT on that job. So i want a good suggestion to avoid the PWHT. What abt inconel welding? How it satisfies the PWHT requirement. If any one knows... please share with me. I hope i will get a good solutions.

 

Regards,

J.C.Andrews,

QA/QC Engineer,

Doha-Qatar.

 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...