Thursday, October 28, 2010

[MW:0] Supporting PQR for Impact requirements

Dear All, 

I have Qualified PQR for welding P1 Gr 1 To P1 Gr 1 with Impact test at (-) 51°C 
thickness range 2.77 to 11.08 mm.
But now we have to weld P1 Gr 1 to P1 Gr 2. Can I do one more supporting PQR with with P1 Gr 1 to P1 Gr 2 With only impact testing.
Please clarify whether Tensile test and bend test are mandatory for supporting  PQR.


Thanking you.
atul chaturvedi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...