You have not specified full details. Assuming that it is all round welding and if have not drilled a hole on the pad for gas to escape it is possible that due to expansion of entapped gas between the pad and the shell , cracks might have developed.


 
On Wed, Sep 30, 2009 at 12:38 AM, bdsathiyamoorthy <bdsathiyamoorthy@gmail.com> wrote:
Dear All,
 
I am doing tank construction. I have found some cracks on the pad toe and pad corner. Shell thk 38 mm, pad thk 30 mm and fillet weld size 21 mm. we were controlled everything. (electorde quiver temp. preheat, oven temp. before start welding good cleaning and etc).
 
Material details :
 
Shell mat'l  : A537 
Pad mat'l   : S275 Gr J
 
Electrode    : E7018
 
Pls any one can sugest to me the causes and prevention.
 
Regards,
Moorthy.
 
 
 
 




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

1 comment:

Suresh Paidi said...

you doesnot specifiy what type of crack that was , We can excute the cause of crack as per the type .

It might be stress concentration .

Suresh
Fluor

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...