Monday, September 28, 2009

[MW:3347] Re: CL in water

I am agree with Mr Kannan,

Wherever such requirements there client specify the chloride content
normally it should not be more than 50ppm for carbon steel job and
25ppm for Stainless steel jos as per my regular experience.

On Sep 28, 8:40 am, GOPU NAIR <gopunair5...@yahoo.com> wrote:
> Dear Kannan
>  
> The extent of Chloride  permitted in water for hydrotesting of SS vessels depends upon the customer specification based on the end use.  Generally customer specifies 25ppm.  In extreme cases they demand choride free (DM) water also. So please follow the customer spec.
>  
> Gopu
>
> --- On Thu, 24/9/09, Kannan <kannan_...@yahoo.com> wrote:
>
> From: Kannan <kannan_...@yahoo.com>
> Subject: [MW:3293] Re: CL in water
> To: "Materials & Welding" <materials-welding@googlegroups.com>
> Date: Thursday, 24 September, 2009, 1:25 AM
>
> In the context of valve pressure test API 6D calls for max. of 30ppm
> chloride for SS and duplex. I do not remember the claus. Pl. have a
> look of the std. At site the piping hydrotest chloride limitation is
> defined in a API RP standard which I am not able to recollect now.
> Moreover having difficulty in achieving such low limits calls for
> relaxation at site overruling such std requirement. 50ppm in such case
> is a limit accepted by most contractors and clients.
>
> regards
> kannan
>
> On Aug 16, 4:18 am, Ali Asghari <asghari...@rocketmail.com> wrote:
>
> > dear all freinds
> > can you share  your expriences about the amount of CL in water that used for hydrostatic testing of st.st?because in somewhere i see 25 ppm and another 50ppm is mentioned.which correct & why?
> > regards
>
>       Yahoo! India has a new look. Take a sneak peekhttp://in.yahoo.com/trynew

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...