For S355 J2 see EN 10025 Part 2 , for this steel Charpy test are carried out at -20°C, delivery condition may be as-rolled or normalised


For S355 G3 see EN 10225 , G3 means that it is a plate with charpy tests at -40°C, delivery condition may be normalised or thermomechanically rolled

They are both C-Mn steels for structural application , S355 j2 is more common while S355 G3 is specifically used for offshore structure or when specific requirements on toughness and weldability are required

Regards


Giorgio Stefano

-----Messaggio originale-----
Da: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Per conto di vipin george
Inviato: sabato 26 settembre 2009 16.53
A: materials-welding@googlegroups.com
Oggetto: [MW:3331] Re: Base Metal

Hi!Noberto,

This is Normalised steel basically for Offshore structures in North sea climatic conditions
S355 J2 means 355 N/mm Sq yield strength , J2 means Impact @ -20 degrees C Avg.Impact value is 27 Joules
S355 K2 G3 means 355 N/mm Sq yield strength , K2 means Impact @ -20 degrees C Avg.Impact value is 40 Joules, G3 means Normalised Killed steel
Check dnv.com, Download this code free:DNV-OS-C401 (Mettalic materials)
SMAW process: E7018 & E7018-1
GMAW process: ER 70S-6
FCAW process: E 71T-1C/ E71T-9C

Thanks & Regards,
vipin george


On Fri, Sep 25, 2009 at 3:10 PM, Norberto Barbosa <norberto.sb@hotmail.com> wrote:


Hi, everybody
Is there someone who knows this kind of Base Material "S-355 J2 G3", regarding;
1)Similarity with ASTM;
2) Quimical Composition
3) and if possible an adequate electrode with its AWS classification and specification to weld this material.
I'll be glad.

Regardings,
Norberto de Souza Barbosa - Brazil






________________________________

Novo Internet Explorer 8: mais rápido e muito mais seguro. Baixe agora, é grátis! <http://brasil.microsoft.com.br/IE8/mergulhe/?utm_source=MSN%3BHotmail&utm_medium=Tagline&utm_campaign=IE8>

******************************************************************************************
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...