Thursday, September 24, 2009

[MW:3303] Re: Welder reapir %

If it is cut and reweld, 100% repair to be considered for quality
costing; but, for welder performance, the actual repair/defect % only
to be considered - this is just a thought....

Thanks
Senthil

On Sep 24, 3:35 pm, Adi <adinr...@gmail.com> wrote:
> If joint repair came in 2" pipe, it is very difficult to identify
> repair the exact location & root repair we can't do, so the joint
> should be cut out
> My question is When we are calculating the welders repair %  we have
> to consider total length of 2" is repair ? Why because we repaired the
> total length
> Is it correct please advice
>
> Adi

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...