In the context of valve pressure test API 6D calls for max. of 30ppm
chloride for SS and duplex. I do not remember the claus. Pl. have a
look of the std. At site the piping hydrotest chloride limitation is
defined in a API RP standard which I am not able to recollect now.
Moreover having difficulty in achieving such low limits calls for
relaxation at site overruling such std requirement. 50ppm in such case
is a limit accepted by most contractors and clients.

regards
kannan

On Aug 16, 4:18 am, Ali Asghari <asghari...@rocketmail.com> wrote:
> dear all freinds
> can you share  your expriences about the amount of CL in water that used for hydrostatic testing of st.st?because in somewhere i see 25 ppm and another 50ppm is mentioned.which correct & why?
> regards

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS