[MW:3239] RE: 3238] Shelf life of Low hydrogen electrodes

Consult the consumable manufacturer, may be shelf life revalidated with additional testing. Code does not specify the shelf life, but the manufacturer does.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ravindra T
Sent: Thursday, September 17, 2009 3:28 PM
To: materials-welding@googlegroups.com
Subject: [MW:3238] Shelf life of Low hydrogen electrodes

 

Dear All

 

Our contractor has brought low hydrogen electrodes (E 7018 & 8018) which are manufactured in 2007 for welding station piping in one of our intermediate pump station of our cross country pipeline project. I would like to know whether these electrodes can be used now?. Is there any reference in ASME code regarding the expiry/ shelf life of Electrodes?

 

Please advise me in this regard.

 

Thanking you all in advance

 

Ravindra

Senior Project Engineer




--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...