[MW:3234] pickling procedure for c.s piping



dear all:
 
we are going to apply pickling on carbon steel piping due to high iron content observed in service, so i would like to know the procedure and steps to be followed ,i would appreciate if any one have aprocedure applied before or any specs for any company discuss this issue.
 
thanks in advance
A.eissa
QC engineer


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---