"P" stands for piping. Please refer SA234, in which the scope elaborate the type of fitting. Gopu
--- On Tue, 15/9/09, saqib gul <saqibgul@gmail.com> wrote:
From: saqib gul <saqibgul@gmail.com> Subject: [MW:3207] Re: 3193] Valves A-216 WCB To: materials-welding@googlegroups.com Date: Tuesday, 15 September, 2009, 9:30 AM
And what WPB means for fittings? On Mon, Sep 14, 2009 at 7:13 PM, John Henning <jhenning@deltak.com> wrote: weldable casting (carbon steel) grade B We use valves specification e.g. Gate valve, cast steel, ASTM A-216 Grade WCB, Class 150, Flanged ANSI B 16.34 My question is what does "WCB" stands for? If it is a grade of A-216 but what does it exactly mean? If some one know it's abbreviation?
See the Web's breaking stories, chosen by people like you. Check out Yahoo! Buzz --~--~---------~--~----~------------~-------~--~----~ To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. -~----------~----~----~----~------~----~------~--~---
Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP -- https://materials-...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
|
1 comment:
a 216 is carbon steel casting material. wcb stands welded cat (not sure) b stands for grade b