Dear Dayalan,
You need to carry out procedure using P5B material only. deviation not permited
 
amarjit singh

On Tue, Sep 8, 2009 at 6:39 PM, Harikumar Dayalan / ZS Saudi PED QA/QC <harikumar@zamilsteel.com> wrote:

Dear Friends

 

I need to qualify procedures for P5B (9Cr-1MoL) material urgently, at present I don't have any material in stock

 

Since the preheat, interpass, interpass stress relieving and post weld temperature for P5B are too maintained strictly.

 

is the procedure qualification is  possible by buttering? Did the secIX and Sec VIII Accepts.

 

Did anybody done it, if so how about the mechanical test results.

 

 

Regards

Harikumar Dayalan

  

 


--------------------------------------------------------------------------------------------------------
Disclaimer: This email and any files transmitted with it are confidential
and intended solely for the use of the addressee(s) named herein. If you
are not the intended recipient or addressee, you should not use, disseminate,
distribute, copy or alter this email. Any views or opinions presented in this
email are solely those of the author and might not represent those of "Zamil
Industrial" and or its units.

Warning: Although reasonable precautions have been taken to ensure no viruses
are present in this email, the company cannot accept responsibility for any
loss or damage arising from the use of this email or attachments. If you have
received this electronic mail message in error, please contact the sender directly.




--
Amarjit Singh

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...