[MW:3189] Re: Ferrite limits

It all depends on the customer spec. Generally (theoritically) minimum 3% to max 12% is acceptable. But depends on the criticality client restric the limit of max ferrite.

2009/9/13 ma <azizi-m@pidec.com>

Hi every body
what is the acceptable criteria of Ferrite phase during the Stainless
Steel weding?

Thanks
MA





--
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...